Skip to main content

Table 1 Lattice parameter, crystallite size, peak width, and strain variation for undoped and Cu-doped films

From: Synthesis and characterization of Cu-Doped ZnO nanostructures for UV sensing application

Cu ratio

a (Å)

c (Å)

d002 (Å)

D (nm)

FWHM

εc (%)

εa (%)

0%

3.24686

5.20312

2.610

29.7

0.280

0.06

− 0.097

5%

3.24686

5.20312

2.602

26.7

0.298

0.06

− 0.097

7%

3.25549

5.21137

2.606

31.05

0.257

0.218

0.169

9%

3.25674

5.22268

2.611

31.8

0.250

0.436

0.207

11%

3.26192

5.21902

2.610

23.4

0.340

0.365

0.367

15%

3.25488

5.21228

2.606

20.5

0.388

0.236

0.150